Oxide

...from spray roaster and fluidised bed

 

We offer profitable marketing for the oxide produced by the regeneration process. We also offer technologies to improve the quality of oxide in order to achieve profitable prices on the world market respectively to improve the handling of the oxide..

 

Fluidised Bed Oxide
Particle size: 0,2 - 2 mm
Specific surface: < 1 m2 / g
Bulk density: 3,8 kg / dm3
   Sprayroast Oxide
Particle size: 30 - 40 µm
Specific surface: 3 - 5 m2 / g
Bulk density: 0,4 - 0,6 kg / dm3

 

To produce oxide which meets the demands of the market, it is especially important to reduce the silicon content, minimise the chlorine content and maximise the specific surface.